| Customization: | Available |
|---|---|
| Type: | Special Steel Bar |
| Standard: | AISI, ASTM, DIN, JIS, GB, BS |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
1.2714/L6/Skt4 Mold building bar corten High satisfaction Tool Steel with Factory Price
DIN1.2714 Tool Steel for Hot Forging Die or Plastic Mould

Equivalence
| AISI / SAE | DIN / W.Nr | JIS | GB |
| L6 | 1.2713 / 1.2714 | SKT4 | 5CrNiMoV |
Chemical Composition(%)
| Steel Grade | C | Si | Mn | P | S | Cr | Mo | V | Ni |
| 1.2714 | 0.50-0.60 | 0.10-0.40 | 0.60-0.90 | ≤ 0.030 | ≤ 0.030 | 0.80-1.20 | 0.35-0.55 | 0.05-0.12 | 1.50-1.80 |
| 1.2713 | 0.50-0.60 | 0.10-0.40 | 0.65-0.95 | ≤ 0.030 | ≤ 0.030 | 0.60-0.80 | 0.25-0.35 | 0.07-0.12 | 1.50-1.80 |
| L6(AISI) | 0.65-0.75 | 0.10-0.50 | 0.25-0.80 | ≤ 0.030 | ≤ 0.030 | 0.60-1.20 | ≤ 0.50 | -- | 1.25-2.00 |
| 5CrNiMoV | 0.50-0.60 | ≤ 0.40 | 0.50-0.80 | ≤ 0.030 | ≤ 0.030 | 1.00-1.20 | 0.45-0.55 | 0.07-0.12 | 1.40-1.80 |
| SKT4(JIS) | 0.50-0.60 | ≤ 0.35 | 0.60-1.00 | ≤ 0.030 | ≤ 0.030 | 0.70-1.00 | 0.20-0.50 | -- | 1.50-1.80 |
Supply Specifications
| Condition | Processing Route |
Tolerance Range |
Surface Quality |
Application Notes |
| Black | / | Rolled: +3~5 mm Forged: +10~20 mm |
Hot-rolled black scale surface | Economical choice for large volume orders |
| Rough Machined |
Milled 4 sides + Rough ground 2 sides
|
Rolled: +0~1 mm Forged: +0~5 mm |
Clean surface no heavy scale |
Pre-machined surface ready for further processing |
| Fully Machined |
6 sides precision milled + ground |
+0.05~0.1 mm | Surface roughness Ra1.6 | Ready for direct CNC machining |
| Ground Finish |
6 sides fine ground | +0.02~0.05 mm |
Mirror finish
|
For high-precision molds |
| Custom cutting service available according to drawings | ||||

Annealing
650 to 700°C
Slow controlled cooling in furnace at a rate of 10 to 20°C/hr (50 to 68°F/hr) down to approx. 600°C, (1112°F) further cooling in air.
Hardness after annealing: max. 248 HB.
Stress relieving
Approx. 650°C
Slow cooling in furnace; intended to relieve stresses set up by extensive machining, or in complex shapes. After through heating, hold in neutral atmosphere for 1 - 2 hours.
Tempering
Slow heating to tempering temperature im- mediately after hardening / time in furnace 1 hour for each 20 mm of workpiece thickness but at least 2 hours / cooling in air. It is recommended to temper at least twice.
A third tempering cycle for the purpose of stress relieving may be advantageous.
• Stable supply from leading domestic and overseas tool steel mills
• Complete tool steel grade portfolio
• Competitive pricing advantage
• Large stock and flexible cutting services
• Flexible delivery and supply solutions
• Professional technical support